The microhardness HV0.1 of special titanium carbide powder for thermal spraying reaches 3000-3800.Low friction coefficient, low density,is an excellent self-lubrication,oxidation resistance, corrosion resistance,high temperature resistant material.It can resist the high temperature of 3000 degrees and has excellent wear resistance.
It is used for thermal spraying, PTA spray welding and PTA surfacing on the workpiece surface with high temperature resistance,corrosion resistance and wear resistance.
| Medium/Fine Grain Size | |||||||||
| Grade | Chemical Contents(%) | particle
size (um) |
|||||||
| Total Carbon
(T.C.) |
Free Carbon (F.C.) |
Impurity Contents(<=%) | |||||||
| Si | Al | O | N | Na | Ca | ||||
| TiC-3 | >19.0 | <0.35 | 0.05 | 0.01 | 0.4 | 0.5 | 0.01 | 0.02 | 75-150 |