TiC titanium carbide powder material, molecular formula: TiC, gray-black powder, is a metallic gray iron-gray crystal. At the lattice position, carbon atoms are equivalent to titanium atoms, and TiC atoms are strongly covalently bonded, NaCl Type cubic crystal structure, lattice constant is 0.4329 nm, space group is Fm3m, theoretical density is 4.9g/cm3, melting point is 3160°C, boiling point is 4300°C, thermal conductivity is 24.28[W(m·K)-1](20 °C), resistivity 52×10-6Ω·cm, microhardness 3000KG·mm-2, thermal expansion coefficient 6.73×10-6/°C, resistivity 40~50/μΩ·cm, elastic modulus 46×103MPa, The compressive strength is 1380 MPa.
TiC titanium carbide powder material is a typical transition metal carbide with good chemical stability, high temperature resistance, high wear resistance, high melting point, high hardness, hardness second only to diamond, good thermal conductivity and electrical conductivity, it exhibits superconductivity even at very low temperatures. Titanium carbide can form binary, ternary, quaternary, pentad, and hexavalent compound solid solution with rare earth carbides such as tungsten carbide, tantalum carbide, tantalum carbide, chromium carbide, titanium nitride, zirconium carbide, and tantalum carbide, which can improve alloy material’s red hardness, wear resistance, oxidation resistance and corrosion resistance.
| Grade | Chemical Contents(%) | particle
size (um) |
|||||||
| Total Carbon
(T.C.) |
Free Carbon (F.C.) |
Impurity Contents(<=%) | |||||||
| Si | Al | O | N | Na | Ca | ||||
| TiC-2 | >19.0 | <0.40 | 0.05 | 0.01 | 0.5 | 0.6 | 0.01 | 0.02 | 3-10 |
Note: We can make the different particle size and chemical composition according to customize.
| Grade | Chemical Contents(%) | particle
size (um) |
|||||||
| Total Carbon
(T.C.) |
Free Carbon
(F.C.) |
Impurity Contents(<=%) | |||||||
| Si | Al | O | N | Na | Ca | ||||
| TiC-1 | >19.0 | <0.40 | 0.05 | 0.01 | 1.0 | 0.5 | 0.01 | 0.02 | 0.8-1.5 |
| TiC-2 | >19.0 | <0.40 | 0.05 | 0.01 | 0.5 | 0.6 | 0.01 | 0.02 | 3-10 |
| TiC-3 | >19.0 | <0.35 | 0.05 | 0.01 | 0.4 | 0.5 | 0.01 | 0.02 | 75-150 |
| TiC-4 | >15 | <0.3 | 0.05 | 0.01 | 0.3 | 0.4 | 0.01 | 0.02 | 1000-4000 |
Note: We can make the different particle size and chemical composition according to customize.
Production Process and Product Quality Technical Standards:

Product application case:
Adding 6-30% TiC titanium carbide powder material to the tungsten carbide-cobalt cemented carbide can form a titanium carbide-tungsten carbide solid solution, which can improve the red hardness, wear resistance, oxidation resistance and corrosion resistance of the alloy. It is more suitable for processing steel than WC-Co cemented carbide. It is widely used in cemented carbide cutting tool products; it is applied to alloys such as Ni-Mo as binders to make tungsten-free hard alloys, which can improve the turning speed and the precision and smoothness of the workpieces. Used as an additive to make thermistors, improving their electrical conductivity and wear resistance.